GB standards are the China national standards; Prefix code GB are Mandatory standards, GB/T are Recommended standards; All products or service must be compliance with GB standards; If you want to export products or services to huge Chinese market, need ensure they are meet the requirements of GB china national standards;  We provide Chinese GB standards and English version GB standards  Lookup, Translate, Download, Imported Commodity GB standards Testing and Compliance review services.
  •  China "superalloys" GB Standards List:
  • Standard  Code GB Standard Title Standard Class Order
  • GB/T 31309-2014
  • Calculation of electoron vacancy number in nickel-base superalloys superalloys
    China National Standards
  • GB/T 14999.3-2012
  • Test methods for superalloys - Part 3: Verification of longitudinal fracture of bars superalloys
    China National Standards
  • GB/T 14999.1-2012
  • Test method for superalloys - Part 1: Verification of longitudinal macro-structures and defect by etch superalloys
    China National Standards
  • GB/T 14999.4-2012
  • Test methods for superalloys - Part 4: Determination of characterizing banding grains and primary carbides distribution of superalloy rollings superalloys
    China National Standards
  • GB/T 14999.2-2012
  • Test methods for superalloys - Part 2: Verification of transverse macro-structures and defect by etch superalloys
    China National Standards
  • GB/T 14992-2005
  • Classification and designation for superalloys and high temperature intermetallic materials superalloys
    China National Standards
  • GB/T 14999.5-1994
  • Photomicrographs and photomacrographs for evaluating of heat-resisting superalloys superalloys
    China National Standards

    Find out:7Items   |  To Page of: First -Previous-Next -Last  | 1

     

    +86-400-6578191        info@transcustoms.com 
    106# Zhongmao Mansion,No.1 Beizhan Road,Shenzhen,China
    ©  RJS Copyright  2001-2018 All Rights Reserved

    - Since 2001 -
    Focus on China Standards & Compliance Services

    www.rjs.cn

    China Licenses

    www.transcustoms.com

    China HS code & Tariff

    www.gbstandards.org

    China National Standards